ASTM B409 Haynes HR120 Nickel Alloy

ASTM B409 Haynes HR120 Nickel Alloy

Haynes HR-120 is a solid solution strengthened nickel-iron alloy. It offers high temperature resistance, high strength, and excellent resistance to carburization and sulfidation environments. It is an ideal material for industrial heat treatment equipment.
Enviar la consulta

 

ASTM B409 Haynes HR120 Nickel Alloy Description

 

Lork Group supplies ASTM B409 Haynes HR120 Nickel Alloy in the annealed state. Strips are available in two standards: ASTM B408 and ASTM B409. Typical specifications include thicknesses of 3mm to 16.0mm and widths of 30mm to 3000mm. Special strip sizes (thicknesses of 0.02mm to 3mm, widths of 5mm to 30mm) vary significantly in price. Please contact us if you require this product.

 

 

1. Price Reference

 

The price of high-performance alloys is significantly affected by raw material market prices, product form (e.g., strip, plate), specifications, quantity, and supplier channels, and can fluctuate significantly. Lork Group's prices (e.g., $30-35/kg for a 50kg MOQ / $25-30/kg for 100-300kg) are for reference only. Please ensure you inquire with us for real-time price comparisons.

 

2. Purchasing Recommendations

 

Confirm material performance requirements based on your application environment (temperature, media). When purchasing, ensure that the material complies with relevant standards (such as ASTM B409) and request a complete Material Certificate (MTC).

 

Based on your subsequent processing, determine the required material supply condition (e.g., solution annealed).

 

ASTM B409 Haynes HR120 Nickel Alloy Parameters

 

 

 Haynes HR120 Nickel Alloy Custom

Lork Group is rooted in "Global Craftsmanship, Intelligent Manufacturing in China," with full-process quality control as the core, and rigorously selected suppliers. We professionally craft nickel alloys for you!.
ASTM F408 Haynes HR120 Nickel Alloy rod

Haynes HR120 Bar

UNS N08120
ASTM B408
Haynes HR120 Nickel Alloy plate

Haynes HR120 Plate

UNS N10665
W.Nr. 2.4617
ASTM B333
Haynes HR120 Nickel Alloy pipe

Haynes HR120 Pipe

UNS N08120
ASTM B515/B163
ASTM F408 Haynes HR120 Nickel Alloy

Haynes HR120 Strip

UNS N08120
ASTM B366
ASTM B564

 

Haynes HR120 Nickel Alloy Manufacturing and Pricing Reference

 

 

Haynes HR120 Nickel Alloy Strip

   The alloy is typically supplied in the solution annealed condition, annealing temperatures ranging from 1177-1210℃ (2150-2210℃F) followed by rapid cooling.

Hot/Cold Forming: The alloy is readily cold or hot formable.

Welding: Haynes 556 filler wire is typically used for welding.

ASTM B409 Haynes HR120 Nickel Alloy. The approximate prices by Lork Group are:

1. Processing: Cutting, chipping, milling, etc. (Price based on material loss and processing method)
2. Custom Material - Metallurgy, heat treatment, and other solutions available (Price based on your requirements)

 susan@lorkgroup.com
 +86 19937075488

Haynes HR120 Nickel Alloy

 

 The above prices are average market prices for materials and are for reference only. For real-time pricing, please send us your order request for more information! 

 

 

Haynes HR120 Nickel Alloy Chemical Composition

 

 

Haynes HR120
<= 1.50
23.0 - 27.0
<= 2.50
W <= 2.50
<= 3.0
35.0 - 39.0

 

 

Haynes HR120 Nickel Alloy Mechanical Properties

 

 

Haynes HR120
>= 621 MPa
375 MPa
50%
197 GPa

 For more Haynes HR120

 